POTASSIUM TITANATE CAS#12030-97-6

POTASSIUM TITANATE CAS#12030-97-6

Excellent High-Temperature Resistance: Potassium titanate can withstand temperatures up to 1200°C, making it suitable for high-temperature industrial applications.


Low Thermal Conductivity: It has low thermal conductivity, which helps provide effective thermal insulation performance.


High Infrared Reflectivity: The material exhibits strong infrared reflectivity, supporting applications in heat management and thermal protection.


Strong and Stable Crystal Structure: With a needle-like crystal morphology and Mohs hardness of 4, potassium titanate offers good mechanical stability and durability.



WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of ‌POTASSIUM TITANATE CAS#12030-97-6

Potassium titanate is an inorganic compound composed of potassium oxide and titanium dioxide with the general formula K₂O·nTiO₂ (n=1,2,4,6,8). It is a white solid with a relative density of 3.1 and a melting point of 1515℃, forming a strongly alkaline solution when reacting with water. It mainly exists in two crystal forms: potassium tetratitanate (K₂Ti₄O₉) and potassium hexatitanate (K₂Ti₆O₁₃). It presents white needle-like crystals with a Mohs hardness of 4, featuring low thermal conductivity, high infrared reflectivity and high temperature resistance up to 1200℃.


Product Application of POTASSIUM TITANATE CAS#12030-97-6

It can be used as thermal insulation material, electrical insulation material, catalyst carrier and filter material. As a friction material, it reduces friction by about 50% and wear by around 32% compared with asbestos, suitable for brakes, clutches and other friction parts. After surface modification with Sb/SnO₂ to gain conductivity, it can be used as conductive material or blended with plastics to make conductive composites. It also serves as ion exchange material and adsorbent.


Product Information

Parameters


Melting point1615°C
density3.1
solubilityreacts with H2O
formPowder
colorwhite orthorhombic crystals, crystalline
Water Solubilityhydrolyzes in H2O to give a strongly alkaline solution [HAW93]
CAS DataBase Reference12030-97-6(CAS DataBase Reference)
EPA Substance Registry SystemPotassium titanium oxide (K2TiO3) (12030-97-6)
Safety Statements22
WGK Germany3
TSCATSCA listed


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products