Strontium Carbonate CAS#1633-05-2

Strontium Carbonate CAS#1633-05-2

High-Quality Industrial Grade:Produced with reliable purity, ensuring consistent performance across various industrial applications.


Naturally Derived:Sourced from the mineral strontianite, providing a stable and dependable raw material.


Versatile Applications:Suitable for use in multiple industries, including pyrotechnics, ceramics, and electronics.


Cost-Effective Red Colorant:Widely used in pyrotechnics for producing bright red flames, offering an economical solution for flame coloration.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Strontium Carbonate CAS#1633-05-2

Strontium carbonate (SrCO₃,CAS#1633-05-2) is a carbonate salt of strontium,naturally occurring as the mineral strontianite.It finds applications across a variety of industries.Currently,strontium carbonate is commonly used as a cost-effective colorant in pyrotechnics,as strontium and its salts produce a bright red flame.


Product Application of Strontium Carbonate CAS#1633-05-2

Strontium carbonate (SrCO₃) is widely used in pyrotechnics and ceramic ferrites.It is also applied in the production of iridescent glass for color television tubes.Additionally,it finds use in sugar refining and the preparation of other strontium salts.Its most common application is as a cost-effective colorant in fireworks.

Product Information

Parameters


Melting point1494 °C (lit.)
density3.7 g/mL at 25 °C (lit.)
refractive index1.518
storage temp.Inert atmosphere,Room Temperature
solubilitydilute aqueous acid: slightly soluble(lit.)
formPowder
colorwhite
Specific Gravity3.7
OdorOdorless
PH7-8 (20°C, 0.01g/L in H2O)
Water SolubilitySoluble in ammonium chloride. Slightly soluble in ammonia and water.
Merck148,838
Solubility Product Constant (Ksp)pKsp: 9.25
Stability:Stable. Incompatible with strong acids.
InChIKeyLEDMRZGFZIAGGB-UHFFFAOYSA-L
LogP-0.809 (est)
CAS DataBase Reference1633-05-2(CAS DataBase Reference)
EPA Substance Registry SystemCarbonic acid, strontium salt (1:1) (1633-05-2)


Safety Information


WGK Germany-
TSCAYes
HS Code2836920000
Hazardous Substances Data1633-05-2(Hazardous Substances Data)


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products