Manganese Sulfate Monohydrate CAS#10034-96-5

Manganese Sulfate Monohydrate CAS#10034-96-5

High Bioavailability of Manganese:Provides an easily absorbable source of manganese, making it ideal for nutraceutical, dietary supplement, and feed applications.


Stable Monohydrate Crystal FormThe monohydrated structure ensures good stability, consistent composition, and reliable handling during storage and processing.


Versatile Nutritional and Industrial UseWidely applied in nutraceuticals, animal nutrition, agriculture, and industrial formulations as an essential trace mineral source.


Efficient Manganese CarrierActs as an effective manganese delivery compound, supporting plant growth, animal health, and various biochemical and manufacturing processes.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Manganese Sulfate Monohydrate CAS#10034-96-5

Manganese(II) Sulfate Monohydrate is the monohydrate of manganese sulfate with one crystal water molecule. It is an important manganese-based inorganic compound, commonly used as a nutraceutical and nutritional manganese supplement source. As a hydrated manganese salt, it acts as a key manganese and sulfate carrier, supplying bioavailable manganese for food, agricultural and industrial uses.


Product Application of Manganese Sulfate Monohydrate CAS#10034-96-5

Manganese Sulfate Monohydrate is widely used as a colorant in dyes, fertilizers, animal feed additives and red porcelain glazes. It is also applied in paints and ceramics production, and serves as a reliable manganese source in nutrient formulations and dietary supplements. In industrial processing, it is vital for manufacturing manganese dioxide, and acts as a key precursor for producing metallic manganese and other manganese compounds.

Product Information

Parameters


Melting point700 °C
Boiling point850 °C
bulk density1000-1200kg/m3
density2.95
refractive index1.508-1.522
storage temp.Store at +15°C to +25°C.
solubility5-10 g/100 mL at 21°C
formSolid
colorPink
OdorOdorless
PH3.0-3.5 (50g/l, H2O, 20℃)
Water SolubilityProduct Application of  HydroquinoneCAS#123-31-95-10 g/100 mL at 21 ºC
SensitiveHygroscopic
Merck145,739
Exposure limitsACGIH: TWA 0.02 mg/m3; TWA 0.1 mg/m3
OSHA: Ceiling 5 mg/m3
NIOSH: IDLH 500 mg/m3; TWA 1 mg/m3; STEL 3 mg/m3
InChIKeyISPYRSDWRDQNSW-UHFFFAOYSA-L
LogP-1.031 (est)
CAS DataBase Reference10034-96-5(CAS DataBase Reference)
EPA Substance Registry SystemManganese(II) sulfate monohydrate (10034-96-5)


Safety Information


Hazard CodesXn,N
Risk Statements48/20/22-51/53
Safety Statements22-61
RIDADRUN 3077 9/PG 3
WGK Germany1
RTECSOP0893500
F3
TSCAYes
HazardClass9
PackingGroupIII
HS Code28332990
ToxicityLD50 orally in Rabbit: 2150 mg/kg


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products