Melamine CAS#108-78-1

›

‹

›

Melamine CAS#108-78-1

High Purity White Crystalline Form: Melamine is a white crystalline compound with a defined chemical structure, making it suitable for precise industrial applications.


Unique Triazine Ring Structure: Its six-membered ring of alternating carbon and nitrogen atoms with three amino groups provides chemical stability and reactivity for various syntheses.


Versatile Polymerization Capability: Melamine can be copolymerized with methanal to form thermosetting melamine resins, enabling its use in durable and heat-resistant materials.


Widely Used in Laminated Coatings: The resulting melamine resins are particularly valuable for laminated coatings, offering strong adhesion, hardness, and resistance to wear and chemicals.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Melamine CAS#108-78-1

Melamine is a trimer of cyanamide featuring a 1,3,5-triazine ring structure. It functions as a xenobiotic metabolite and is chemically related to cyanamide, serving as the conjugate base of melamine(1+).

Melamine (C₃N₆H₆) is a white crystalline compound with a cyclic six-membered ring composed of alternating carbon and nitrogen atoms, bearing three amino (NH₂) groups. It can be copolymerized with methanal to produce thermosetting melamine resins, which are widely used in laminated coatings.


Product Usage

Melamine is widely used in the production of high-pressure laminating resins, such as decorative countertops, molded compounds like dinnerware, and surface coating resins for appliances and automotive topcoats. It is also utilized in textile and paper treatment resins. Other applications include adhesive resins for bonding lumber, plywood, and flooring, as well as resins used in leather tanning. Melamine, melamine cyanurate, other melamine salts, and guanidine compounds are among the most commonly used nitrogen-containing flame retardants. Specifically, melamine serves as a flame retardant additive for polypropylene and polyethylene, while melamine cyanurate is commercially applied as a flame retardant for polyamides and terephthalates.


Product Information

Parameters

Product Name:Melamine
Synonyms:2,4,6-TRIAMINO-1,3,5-TRIAZINE FOR SYNTHE;1,3,5-Triazine-2,4,6-triamine (Melamine);MELAMINE(P);Melamine, synthesis grade;Melamine 5g [108-78-1];Melamine,2,4,6-Triamino-1,3,5-triazine, sym-Triaminotriazine;Melamine (250 mg) (2,4,6-Triamino-1,3,5-triazine);1,3,5-Triazin-2,4,6-triaMine
CAS:108-78-1
MF:C3H6N6
MW:126.12
EINECS:203-615-4
Product Categories:Building Blocks;Chemical Synthesis;Heterocyclic Building Blocks;Triazines;Amines;Aromatics;Fine chemical;Heterocycles;Organics;Bases & Related Reagents;Nucleotides;108-78-1
Mol File:108-78-1.mol
Melting point>300 °C (lit.)
Boiling point224.22°C (rough estimate)
bulk density800kg/m3
density1.573
vapor pressure66.65 hPa (315 °C)
refractive index1.872
Fp>110°C
storage temp.no restrictions.
solubilitywater: soluble25mg/mL, clear to slightly hazy, colorless
formFine Crystalline Powder
pka5(at 25℃)
colorWhite
PH7-8 (32g/l, H2O, 20℃)
Water Solubility3 g/L (20 ºC)
Merck145811
BRN124341
Stability:Stable. Incompatible with strong acids, strong oxidizing agents. Nonflammable.
InChIKeyJDSHMPZPIAZGSV-UHFFFAOYSA-N
LogP-1.22 at 20℃
CAS DataBase Reference108-78-1(CAS DataBase Reference)
NIST Chemistry Reference1,3,5-Triazine-2,4,6-triamine(108-78-1)
IARC2B (Vol. Sup 7, 73, 119) 2019
EPA Substance Registry SystemMelamine (108-78-1)


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products