Stable and Reliable Properties: Paraffin has stable physicochemical characteristics and a well-defined molecular structure, ensuring consistent performance across a wide range of applications.


Colorless, Odorless, and Tasteless: Its neutral appearance and lack of smell or taste make paraffin especially suitable for medical, food-related packaging, and cosmetic uses.


Cost-Effective and Widely Available: Derived from petroleum distillates, paraffin is inexpensive and readily available, supporting large-scale industrial and commercial applications.


Excellent Thermal Performance: With a large latent heat of phase transition, paraffin is effective for thermal storage, insulation, and temperature-regulating applications in construction and industry.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of ‌Paraffin Wax CAS#8002-74-2

Paraffin is a hydrocarbon blend obtained from specific petroleum distillates, shale oil, or other bituminous mineral oils. It is mainly composed of solid alkanes and is colorless, odorless, and tasteless, typically appearing as a white to light yellow translucent solid. Chemically, paraffin consists of straight-chain saturated alkanes with different molecular weights, following the general formula CₙH₂ₙ₊₂. According to its physical form, paraffin is commonly divided into liquid paraffin, solid paraffin, and microcrystalline paraffin. Owing to its low cost, abundant availability, lack of color and odor, stable physical and chemical properties, and high latent heat of phase change, paraffin is widely applied in fields such as medicine, packaging, construction, military camouflage, industry, and agriculture.

Product Application of Paraffin Wax CAS#8002-74-2

Paraffin wax is used in packaging (paper sizing, waterproof/oil-resistant coating), rubber (antioxidant/release agent), textiles (finishing/batik resist), casting, plastics and electronics. Liquid paraffin serves pharmaceutical applications (non-toxic, bioadhesive-like). Paraffin-based PCMs are used for construction thermal energy storage and military infrared camouflage/decoys.



Product Information

Parameters

English NameParaffin wax
English SynonymsPARAFFIN IN PASTILLE FORM 51-53 PH EUR,B;PARAFFIN IN PASTILLE FORM 52-54 PH EUR,B;PARAFFIN IN B LOCK FORM 42-44 25 KG;PARAFFIN IN BLOCK FORM 46-48 1 KG;PARAFFIN IN PASTILLE FORM 56-58 PH E UR,B;PARAFFIN IN PASTILLE FORM 57-60 PH EUR,B;PARAFFIN IN BLOCK FORM 46-48 25 KG;PARAFFIN IN B LOCK FORM 42-44 1 KG
CAS Number8002-74-2
Molecular FormulaC21H27NO3
Molecular Weight341.44398
EINECS Number232-315-6
Melting point58-62 °C ((ASTM D 87))
Boiling point322°℃
Density0.82 g/mL at 20 °C
Vapor pressure<0.1 hPa (20 °С)
FEMA3216 | PARAFFIN WAX
Refractive indexn20/D 1.45
Flash point113°C
Storage conditionsStore below +30°C
SolubilitySoluble in chloroform, ether, volatile oils, and most warm fixed oils; slightly soluble in ethanol; practically in soluble in acetone, ethanol (95%), and water. Paraffin can be mixed with most waxes if melted and cooled.
FormUltra-low viscosity oil
ColorWhite
pH value7
OdorTasteless
Fragrance typeodorless


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products