Tetrabutyl titanate CAS#5593-70-4

›

‹

›

Tetrabutyl titanate CAS#5593-70-4

High Chemical Purity and Clear Appearance: Tetrabutyl titanate is a colorless to light yellow transparent liquid with stable physical characteristics at room temperature.


Good Compatibility with Organic Solvents: It is easily miscible with common organic solvents such as ethanol and ether, making it suitable for various chemical formulations and processes.


Reactive Hydrolysis Properties: The compound can undergo controlled hydrolysis when exposed to air or moisture, which is useful in many catalytic and material synthesis applications.


Distinct Chemical Characteristics for Industrial Use: With an ester-like odor and reactive titanium structure, tetrabutyl titanate is widely valued in chemical and industrial processes requiring organotitanium compounds.

WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Tetrabutyl titanate CAS#5593-70-4

Tetrabutyl titanate (CAS 5593-70-4) is a colorless to pale yellow transparent liquid with an ester odor. It turns cloudy gradually in air due to hydrolysis. Miscible with ethanol, ether and other organic solvents, it is slightly soluble in water and decomposes readily on contact with water.


Product Application of Tetrabutyl titanate CAS#5593-70-4

Titanium(IV) n-butoxide is widely used to prepare anatase nano-titania powders and ferroelectric bismuth titanate thin films. It also acts as a synthetic intermediate, as well as an additive and processing modifier for paints and coatings. As a TiO₂ precursor, it can synthesize nanocrystalline titanium dioxide at room temperature, and is further applied in dye-sensitized solar cells, photocatalysis and self-cleaning coatings.


Product Information

Parameters


Melting point-55°C
Boiling point206 °C/10 mmHg (lit.)
density1.00 g/mL at 20 °C (lit.)
vapor pressure5.6 hPa (20 °C)
refractive indexn20/D 1.491(lit.)
Fp55 °F
storage temp.Store at +2°C to +8°C.
solubilityMiscible with aliphatic, aromatic, chlorinated and oxygenated solvents.
formLiquid
Specific Gravity0.998
colorPale yellow
explosive limit2.0-12.0%(V)
Water SolubilityRAPIDLY HYDROLIZED
SensitiveMoisture Sensitive
Hydrolytic Sensitivity7: reacts slowly with moisture/water
BRN4148236
Stability:Stable, but moisture sensitive. Flammable. Incompatible with water, moisture, strong oxidizing agents, strong acids.
InChIKeyYHWCPXVTRSHPNY-UHFFFAOYSA-N
LogP0.84 at 25℃
CAS DataBase Reference5593-70-4(CAS DataBase Reference)
NIST Chemistry ReferenceTetrabutoxytitanium(5593-70-4)
EPA Substance Registry SystemTetrabutyl titanate (5593-70-4)


Safety Information


Hazard CodesXi,T
Risk Statements10-36/37/38-67-41-37/38-45
Safety Statements16-26-39-24/25-53
RIDADRUN 1993 3/PG 3
WGK Germany1
RTECSXR1585000
F21
TSCAYes
HazardClass8
PackingGroupIII
HS Code29051900
Hazardous Substances Data5593-70-4(Hazardous Substances Data)
ToxicityLD50 orally in Rabbit: 3122 mg/kg


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products