Aluminum acetylacetonate CAS#13963-57-0

›

‹

›

Aluminum acetylacetonate CAS#13963-57-0

Stable Crystalline Form: Aluminum triacetylacetonate appears as a white crystalline powder with stable physical properties.


Good Solubility in Organic Solvents: It is soluble in various organic solvents such as benzene, toluene, chloroform, ethanol, and diethyl ether, providing flexibility in chemical processing.


Defined Physical Properties for Industrial Handling: The compound has a specific gravity of 1.27 g/cm³, supporting reliable handling and formulation in industrial applications.


Controlled Toxicity Profile: With an oral LD50 of 1000 mg/kg in rats, its toxicity profile is well documented for safe laboratory and industrial use.

WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Aluminum acetylacetonate CAS#13963-57-0

Aluminum triacetylacetonate is a white crystalline powder, sparingly soluble in petroleum ether.

At 25°C, its solubility: water 0.00, methanol 1.8, toluene 14.6, benzene 35.4; also soluble in chloroform, ethanol and diethyl ether.

Rat oral LD50 is 1000 mg/kg. It is classified as UN3467 6.1/PG2 with a specific gravity of 1.27 g/cm³.


Product Application of Aluminum acetylacetonate CAS#13963-57-0

Aluminum acetylacetonate is water-insoluble but freely soluble in organic solvents. It reacts with alkalis, acids and water under high temperature. It is commonly synthesized from aluminum chloride and acetylacetone.


Product Information

Parameters


Melting point190-193 °C(lit.)
Boiling point315 °C(lit.)
density1,27 g/cm3
bulk density500kg/m3
vapor pressure0Pa at 25℃
Fp314-316°C
storage temp.Store below +30°C.
solubility3g/l
formCrystalline Powder
colorWhite to cream
Specific Gravity1.279
PH8 (3g/l, H2O, 20℃)
Water Solubility2.5 g/L (20 ºC)
Hydrolytic Sensitivity4: no reaction with water under neutral conditions
BRN4157942
Stability:Stable. Incompatible with strong oxidizing agents.
InChIKeyKILURZWTCGSYRE-LNTINUHCSA-K
LogP-1.67 at 25℃
CAS DataBase Reference13963-57-0
NIST Chemistry ReferenceAluminum tris(acetylacetonate)(13963-57-0)
EPA Substance Registry SystemAluminum, tris(2,4-pentanedionato-.kappa.O,.kappa.O')-, (OC-6-11)- (13963-57-0)


Safety Information


Hazard CodesXi,Xn
Risk Statements36/37/38-62-52/53-43-41-63
Safety Statements26-36/37/39-61
WGK Germany1
RTECSMO7870000
TSCAYes
PackingGroupIII
HS Code29159000


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products