Bisphenol A CAS#80-05-7

›

‹

›

Bisphenol A CAS#80-05-7

High Purity and Stability:Industrial-grade Bisphenol A has a purity of ≥99% and is chemically stable under normal conditions.


Physical Versatility:It is a white, odorless crystalline solid with well-defined melting (158–159℃) and boiling points (220℃ at 4 mmHg), making it easy to handle and process.


Solubility Flexibility:Soluble in ethanol and acetone, while insoluble in petroleum ether, allowing compatibility with various organic solvents.


Safety in Handling:Low vapor pressure (4.0×10⁻⁸ mmHg at 25℃) reduces inhalation risk, though it should be kept away from strong oxidizing agents and alkalis.



WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of ‌Bisphenol A CAS#80-05-7

Bisphenol A (4,4'-isopropylidenediphenol, ≥99% industrial grade) is a white odorless crystalline solid. Key properties: mp 158–159 °C, bp 220 °C (4 mmHg), vapor pressure 4.0×10⁻⁸ mmHg (25 °C), density 1.195 (20 °C). Slightly soluble in water (0.12 g/L, 25 °C), readily in ethanol/acetone, insoluble in petroleum ether. Stable; avoid strong oxidizers and alkalis.


Product Application of Bisphenol A CAS#80-05-7

Bisphenol A (high-production chemical) is a key raw material for polycarbonate resins (food-contact products) and epoxy-phenolic resins (can coatings). It also acts as an antioxidant and PVC end polymerization inhibitor.

Product Information

Parameters


Melting point158-159 °C(lit.)
Boiling point220 °C4 mm Hg(lit.)
bulk density600kg/m3
density1.195
vapor pressure<1 Pa (25 °C)
refractive index1.5542 (estimate)
Fp227 °C
storage temp.Store below +30°C.
solubility0.12g/l insoluble
pka10.29±0.10(Predicted)
formLiquid
colorClear light yellow to light orange
OdorPhenol like
Water Solubility<0.1 g/100 mL at 21.5 ºC
Merck141,297
BRN1107700
Dielectric constant5.0(20℃)
InChIKeyIISBACLAFKSPIT-UHFFFAOYSA-N
LogP3.4 at 21.5℃
CAS DataBase Reference80-05-7(CAS DataBase Reference)
NIST Chemistry ReferencePhenol, 4,4'-(1-methylethylidene)bis-(80-05-7)
EPA Substance Registry System4,4'-Isopropylidenediphenol (80-05-7)


Safety Information


Hazard CodesXn
Risk Statements37-41-43-62-52
Safety Statements26-36/37/39-45-46-39-36/37-61
RIDADRUN 3077 9 / PGIII
WGK Germany2
RTECSSL6300000
Autoignition Temperature510 °C
TSCAYes
HS Code29072300
Hazardous Substances Data80-05-7(Hazardous Substances Data)
ToxicityLC50 (96 hr) in fathead minnow, rainbow trout: 4600, 3000-3500 mg/l (Staples)


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products