Aluminium phosphate CAS#7784-30-7

›

‹

›

Aluminium phosphate CAS#7784-30-7

High Industrial Purity:Produced with a purity of ≥99%, ensuring consistent quality for industrial applications.


Stable Physical Properties:Exhibits a high melting point of 1800℃ and negligible vapor pressure, providing reliable thermal and storage stability.


Chemical Resistance:Insoluble in water and most common solvents, with very slight solubility in acids, allowing controlled reactivity.


Safe and Stable Handling:Stable under normal conditions and resistant to degradation, though it should be kept away from strong reducing agents for safety.



WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of ‌Aluminium phosphate CAS#7784-30-7

Carboxymethyl cellulose is an industrial-grade product with a purity of ≥99%.It appears as a white,odorless crystalline powder.The compound has a melting point of 1800℃ and decomposes upon boiling.It exhibits negligible vapor pressure at 25℃ and has a relative density of 2.566 at 20℃. This product is insoluble in water,very slightly soluble in hydrochloric acid and nitric acid,and insoluble in ethanol.It is stable under normal conditions but should be kept away from strong reducing agents due to incompatibility.


Product Application of Aluminium phosphate CAS#7784-30-7

Aluminum phosphate is widely used as a flux in ceramics and in the preparation of dental cement,calcium sulfate-silicate cement,and special glasses.It also functions as a pharmaceutical gel. Additionally,it is applied as a catalyst,molecular sieves,emollients,and fire-resistant coatings.In the textile industry,aluminum phosphate serves as an effective anti-fouling agent.

Product Information

Parameters


Melting point1500 °C
density2.56 g/mL at 25 °C (lit.)
storage temp.Inert atmosphere,Room Temperature
solubilityVery slightly soluble in water, practically insoluble in alcohol. It dissolves in dilute solutions of mineral acids and alkali hydroxides.
formPowder
Specific Gravity2.566
colorWhite
Water SolubilityInsoluble
Merck14,358
crystal systemThree sides
Solubility Product Constant (Ksp)pKsp: 20.01
Space groupP3121
Lattice constanta/nmb/nmc/nmα/oβ/oγ/oV/nm30.4942910.4942911.0947619090120
Exposure limitsACGIH: TWA 1 mg/m3
Dielectric constant6.0(Ambient)
InChIInChI=1S/Al.H3O4P/c;1-5(2,3)4/h;(H3,1,2,3,4)/q+3;/p-3
InChIKeyILRRQNADMUWWFW-UHFFFAOYSA-K
SMILES[Al+3].P([O-])([O-])([O-])=O
CAS DataBase Reference7784-30-7(CAS DataBase Reference)
EPA Substance Registry SystemMonoaluminum phosphate (7784-30-7)


Safety Information


Hazard CodesC
Risk Statements34
Safety Statements26-36/37/39-45
RIDADRUN 3260 8/PG 2
WGK Germany1
RTECSTB6450000
TSCATSCA listed
HazardClass8
HS Code28352990
ToxicityLD50 oral in mouse: > 5gm/kg


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products