Lithium Metasilicate CAS#10102-24-6

›

‹

›

Lithium Metasilicate CAS#10102-24-6

High Purity White Powder Form: Available as a white powder or orthorhombic needle crystals, ensuring consistent quality and ease of handling.


Defined Thermal Properties: Features a clear enthalpy of fusion (28.00 kJ/mol), supporting stable and predictable high-temperature performance.


Reliable Manufacturing Process: Produced by fusing lithium carbonate with silicon dioxide (SiO₂), ensuring controlled composition and quality.


Effective Fluxing Agent: Widely used as a flux in glazes and ceramic enamels, improving melting behavior and surface finish in ceramic applications.

WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Lithium Metasilicate CAS#10102-24-6

Lithium metasilicate is white powder or orthorhombic acicular crystal with fusion enthalpy of 28.00 kJ/mol.

It is synthesized by fusing lithium carbonate and silica. Mainly used as flux for ceramic glaze and enamel, it optimizes melting performance and surface finish.


Product Application of Lithium Metasilicate CAS#10102-24-6

Lithium metasilicate is a heat and acid resistant inorganic compound, used as additive for zirconia membranes in membrane separation.

It features high permeability to water vapor and sodium carbonate to boost separation efficiency. It also shows biological activity and clinical application value for medical research use.

Product Information

Parameters


Melting point1204°C
density2,52 g/cm3
refractive index1.584
solubilityinsoluble in cold H2O; reacts with dilute acid
formPowder
colorwhite
Specific Gravity2.52
OdorOdorless
Water Solubilityinsoluble cold H2O, decomposes in boiling H2O [MER06]
Hydrolytic Sensitivity2: reacts with aqueous acid
InChIInChI=1S/2Li.O3Si/c;;1-4(2)3/q2*+1;-2
InChIKeyPAZHGORSDKKUPI-UHFFFAOYSA-N
SMILES[Si]([O-])([O-])=O.[Li+].[Li+]
CAS DataBase Reference10102-24-6(CAS DataBase Reference)
EPA Substance Registry SystemDilithium metasilicate (10102-24-6)
Risk Statements36/37/38
Safety Statements26-36/37/39
WGK GermanyWGK 3
TSCATSCA listed
Storage Class11 - Combustible Solids
Hazard ClassificationsEye Irrit. 2
STOT SE 3


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products