Manganese chloride tetrahydrate CAS#13446-34-9

›

‹

›

Manganese chloride tetrahydrate CAS#13446-34-9

High Purity for Industrial Use:Produced with a purity of ≥99%, ensuring dependable quality and consistent performance in various industrial applications.


Stable Physical and Thermal Properties:Exhibits low vapor pressure and defined thermal characteristics, allowing safe handling, storage, and processing.


Excellent Solubility Performance:Highly soluble in water and soluble in ethanol, enabling easy preparation of solutions for different chemical processes.


Reliable Chemical Stability:Stable under normal conditions with clear compatibility guidelines, supporting safe and controlled use in chemical systems.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Manganese chloride tetrahydrate CAS#13446-34-9

Manganese(II) chloride tetrahydrate is industrial grade with purity ≥99%, presented as pink odorless crystalline powder. It melts at 58℃ with loss of crystal water, and its anhydrous form boils at 1190℃. It has negligible vapor pressure at 25℃ and a relative density of 2.01 at 20℃. It is freely soluble in water, soluble in ethanol, and insoluble in ether. Stable under normal conditions, it should be stored away from strong oxidants and strong bases.


Product Application of Manganese chloride tetrahydrate CAS#13446-34-9

Manganese chloride tetrahydrate is an inorganic reagent widely used in oxidation studies and chemical reactions. It is employed in dyeing, disinfection and natural gas purification. It also acts as a drier for linseed oil and serves as a raw material for electric battery production.

Product Information

Parameters


Manganese chloride tetrahydrate Chemical Properties58 °C(lit.)
Boiling point1190 °C
density2,01 g/cm3
bulk density1150kg/m3
storage temp.Store at +5°C to +30°C.
solubilityH2O: 0.5 M at 20 °C, clear, colorless
formSolid
colorRed
Specific Gravity2.01
PH3.5-6 (50g/l, H2O, 25℃)
PH Range4月6日
Odor ThresholdOdorless
Water Solubility1980 g/L (20 ºC)
SensitiveHygroscopic
λmaxλ: 260 nm Amax: 0.01
λ: 280 nm Amax: 0.01
Merck145,728
Exposure limitsACGIH: TWA 0.02 mg/m3; TWA 0.1 mg/m3
OSHA: Ceiling 5 mg/m3
NIOSH: IDLH 500 mg/m3; TWA 1 mg/m3; STEL 3 mg/m3
Stability:Stable. Incompatible with moisture, strong acids, sodium, potassium, zinc.
InChIKeyCNFDGXZLMLFIJV-UHFFFAOYSA-L
LogP-1.380 (est)
CAS DataBase Reference13446-34-9(CAS DataBase Reference)
EPA Substance Registry SystemManganese chloride (MnCl2), tetrahydrate (13446-34-9)


Safety Information


Hazard CodesXn,Xi
Risk Statements22-52-48/22
Safety Statements61-45-24/25
RIDADRUN 3077 9 / PGIII
WGK Germany1
RTECSOO9650000
F3
TSCAYes
HS Code2827 39 85
HazardClass6.1
PackingGroupIII
ToxicityLD 50 in rats (mmole/kg): 7.5 orally; 0.70 i.p. (Holbrook)


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products