Polyvinyl Chloride Paste Resin CAS#9002-86-2

›

‹

›

Polyvinyl Chloride Paste Resin CAS#9002-86-2

Ultra-Fine Particle Size: PVC paste resin features extremely small primary particles (0.2–2 μm) and finished particle sizes of 30–80 μm, ensuring uniformity and excellent processing performance.


Excellent Dispersibility in Plasticizers: The resin can easily break down into primary particles when mixed with plasticizers, forming a smooth and stable paste, which is ideal for coating and molding applications.


Stable Paste Formation: When dispersed, it creates a consistent, paste-like fluid with good stability, supporting precise processing and high-quality end products.


High Processing Versatility: Its fine powder form and paste-forming ability make it suitable for a wide range of applications requiring controlled viscosity and smooth surface finishes.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Products Description of Polyvinyl Chloride Paste Resin CAS#9002-86-2

Polyvinyl chloride (PVC) is a widely used thermoplastic polymer made from vinyl chloride monomers. Key properties: white-light yellow powder, density 1.35–1.40, chlorine content 56–58%, mp 70–85 °C, excellent chemical resistance, poor thermal/light stability. Available in plasticized soft and unplasticized rigid grades. Used in pipes, wire insulation, films, construction materials and consumer goods.


Product Application of Polyvinyl Chloride Paste Resin CAS#9002-86-2

PVC is a cost-effective, versatile plastic requiring performance-specific additives. Rigid grades are used in chemical equipment, construction and agriculture; flexible grades in wires, cables, films and consumer goods. Additional applications include foam insulation, artificial leather, thermoplastic elastomer seals and chlorofibers (with reported therapeutic benefits for arthritis).

Product Information

Parameters

Melting point170-195 °C (decomp)
Boiling point0.100 °C
density1.4 g/mL at 25 °C (lit.)
Tg85
refractive indexn 1.54
Fp736
storage temp.2-8°C
formpowder
Specific Gravity1.385
colorWhite to Off-White
Dielectric constant3.4(Ambient)
Stability:Stable. Combustible. Incompatible with strong oxidizing agents.
InChIInChI=1S/C2H3Cl/c1-2-3/h2H,1H2
InChIKeyBZHJMEDXRYGGRV-UHFFFAOYSA-N
SMILESC=CCl
Surface tension41.5mN/m at 20°C
CAS DataBase Reference9002-86-2(CAS DataBase Reference)
NIST Chemistry Referencepoly(vinyl chloride)(9002-86-2)
IARC3 (Vol. 19, Sup 7) 1987
EPA Substance Registry SystemPolyvinyl chloride (9002-86-2)



Safety Information


Hazard CodesXi
Risk Statements36/37/38
Safety Statements26-36/37-61
WGK Germany3
RTECSKV0350000
TSCATSCA listed
HS Code3904220000
Hazardous Substances Data9002-86-2(Hazardous Substances Data)

Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products