Tetrachloroethylene CAS#127-18-4

›

‹

›

Tetrachloroethylene CAS#127-18-4

High-Performance Industrial Solvent:Tetrachloroethylene is widely used as an effective industrial solvent and as a cooling and insulating liquid in electrical transformers, delivering reliable performance in demanding applications.


Safe Non-Flammable Properties:This colorless, volatile liquid is nonflammable and features a mild ether-like odor, providing improved safety and ease of handling compared with many organic solvents.


Excellent Thermal & Chemical Stability:With strong resistance to heat and chemical reactions, tetrachloroethylene maintains stable performance in high-temperature and electrically sensitive environments.


Advanced Industrial Production Technology:Manufactured mainly through high-temperature chlorinolysis of light hydrocarbons, tetrachloroethylene offers consistent quality suitable for large-scale industrial use.


WhatsApp : +86 15965632259
Email : admin@luxichemistry.com
Inquiry Now >>

Product Description

Product Description of Tetrachloroethylene CAS#127-18-4

Tetrachloroethylene is a chlorinated hydrocarbon with the molecular formula Cl₂C=CCl₂, widely used as an industrial solvent and as a cooling and insulating liquid in electrical transformers. It appears as a colorless, volatile liquid with a mild ether-like odor and is nonflammable, providing enhanced safety in industrial environments.

Most tetrachloroethylene is produced through high-temperature chlorinolysis of light hydrocarbons, ensuring stable supply and consistent product quality for large-scale industrial applications.


Product Application of Tetrachloroethylene CAS#127-18-4

Tetrachloroethylene (PCE) is also known as perchloroethylene, tetrachloroethene, and 1,1,2,2- tetrachloroethene and is also commonly abbreviated to PER or PERC. Tetrachloroethylene is a volatile, chlorinated organic hydrocarbon that is widely used as a solvent in the dry-cleaning and textile-processing industries and as an agent for degreasing metal parts. It is an environmental contaminant that has been detected in the air, groundwater, surface waters, and soil (NRC, 2010).


Product Information

Parameters


Melting point-22 °C (lit.)
Boiling point121 °C (lit.)
density1.623 g/mL at 25 °C (lit.)
vapor density5.83 (vs air)
vapor pressure13 mm Hg ( 20 °C)
refractive indexn20/D 1.505(lit.)
Fp120-121°C
storage temp.Store at +2°C to +25°C.
solubilitywater: soluble0.15g/L at 25°C
formLiquid
colorAPHA: ≤10
Odorchloroform-like odor
Odor Threshold0.77ppm
Water SolubilityMiscible with alcohol, ether, chloroform, benzene and hexane. Slightly miscible with water.
FreezingPoint-22.0℃
λmaxλ: 290 nm Amax: 1.00
λ: 295 nm Amax: 0.30
λ: 300 nm Amax: ≤0.20
λ: 305 nm Amax: 0.10
λ: 350 nm Amax: 0.05
λ: 400 nm Amax: 0.03
Merck149,190
BRN1361721
Henry's Law Constant4.97 at 1.8 °C, 15.5 at 21.6 °C, 34.2 at 40.0 °C, 47.0 at 50 °C, 68.9 at 60 °C, 117.0 at 70 °C (EPICS-GC, Shimotori and Arnold, 2003)
Dielectric constant2.5(21℃)
Exposure limitsTLV-TWA 50 ppm (~325 mg/m3) (ACGIH), 100 ppm (MSHA and OSHA); TLV-STEL 200 ppm (ACGIH); carcinogenicity: Animal Limited Evidence.
Stability:Stable. Incompatible with strong oxidizing agents, alkali metals, aluminium, strong bases.
LogP2.53 at 20℃
CAS DataBase Reference127-18-4(CAS DataBase Reference)
IARC2A (Vol. Sup 7, 63, 106) 2014
NIST Chemistry ReferenceTetrachloroethylene(127-18-4)
EPA Substance Registry SystemTetrachloroethylene (127-18-4)
ECETOC JACC REPORTTetrachloroethylene (127-18-4)


Safety Information


Hazard CodesXn,N,T,F
Risk Statements40-51/53-23/25-11-39/23/24/25-23/24/25
Safety Statements23-36/37-61-45-24-16-7
RIDADRUN 1897 6.1/PG 3
WGK Germany3
RTECSKX3850000
Autoignition Temperature260℃
TSCAYes
HazardClass6.1
PackingGroupIII
HS Code29032300
Hazardous Substances Data127-18-4(Hazardous Substances Data)
ToxicityLD50 orally in mice: 8.85 g/kg (Dybing); LC for mice in air: 5925 ppm (Lazarew)
IDLA150 ppm


Factory Showcase

  • 45bd51f3-5148-4a17-90ad-e2b6a39f4653
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Loading and Transport

  • 1
  • 2
  • 3
  • 4
  • 5
  • 6
  • 7
  • 8

Product Inquiry

Submit >>

Related Products